The present disclosure relates to a laser welding method. Japanese Unexamined Patent Application Publication No. 2012-228715 discloses that a plurality of stacked metal plates are irradiated with a laser beam while the laser beam is scanned in a circular shape to weld the plurality of metal plates. SUMMARY The inventors have found the following problem with a laser welding method for irradiating a plurality of stacked metal plates with a laser beam while scanning the laser beam in a circular shape to weld the plurality of stacked metal plates. When a plurality of stacked metal plates are welded in an upright position, if a molten pool becomes larger to a certain extent and an amount of molten metal increases, the thickness of the vertically upper part of the molten pool in the plate thickness direction decreases due to gravity acting on the molten pool. Therefore, there is a risk that a keyhole formed in the molten pool may become too large due to the irradiation of the laser beam, and welding failures such as generation of a hole may occur. The present disclosure has been made in light of such circumstances and provides a laser welding method capable of suppressing the occurrence of welding failures when a plurality of stacked metal plates are welded in an upright position. In an aspect of the present disclosure, a laser welding method for irradiating a plurality of stacked metal plates in an upright position with a laser beam to weld the plurality of stacked metal plates includes: irradiating the plurality of metal plates with the laser beam to form a circular molten pool; and scanning the laser beam once around an outer periphery of the molten pool to enlarge the molten pool, wherein in the enlarging of the molten pool, a scanning start point of the laser beam is set within a range from 135 degrees to 315 degrees in a scanning direction of the laser beam, with 0 degrees directly above the molten pool in a vertical direction. In the laser welding method according to the aspect of the present disclosure, in the scanning of the laser beam once around an outer periphery of the molten pool to enlarge the molten pool, a scanning start point of the laser beam is set within a range from 135 degrees to 315 degrees in a scanning direction of the laser beam, with 0 degrees directly above the molten pool in a vertical direction. In this configuration, when the laser beam is emitted on the vertically upper side of the molten pool, the molten pool is not sufficiently enlarged, and thus the amount of molten metal in the molten pool is small. Therefore, the necking generated on the vertically upper side of the molten pool is small, so that the keyhole formed on the vertically upper side of the molten pool does not become too large. Accordingly, it is possible to suppress the occurrence of welding failures such as generation of a hole. In the enlarging of the molten pool, the scanning start point of the laser beam may be set within a range from 180 degrees to 270 degrees in the scanning direction of the laser beam. With this configuration, it is possible to better suppress the occurrence of welding failures such as generation of a hole. In the enlarging of the molten pool, the vertical direction may be detected by a sensor, and the scanning start point of the laser beam may be determined based on the vertical direction detected by the sensor. This configuration allows the laser welding system to automatically determine the scanning start point of the laser beam. In the enlarging of the molten pool, an irradiation energy density of the laser beam may be reduced more on a vertically upper side of the molten pool than on a vertically lower side of the molten pool. With this configuration, it is possible to better suppress the occurrence of welding failures such as generation of a hole. In another aspect of the present disclosure, a laser welding method for irradiating a plurality of stacked metal plates in an upright position with a laser beam to weld the plurality of stacked metal plates includes: irradiating the plurality of metal plates with the laser beam to form a circular molten pool; and scanning the laser beam once around an outer periphery of the molten pool to enlarge the molten pool, wherein in the enlarging of the molten pool, an irradiation energy density of the laser beam is reduced more on a vertically upper side of the molten pool than on a vertically lower side of the molten pool. In the laser welding method according to the aspect of the present disclosure, in the enlarging of the molten pool, an irradiation energy density of the laser beam is reduced more on a vertically upper side of the molten pool than on a vertically lower side of the molten pool. Therefore, a keyhole formed on the vertically upper side of the molten pool does not become too large, and the occurrence of welding failures such as generation of a hole can be suppressed. In the enlarging of the molten pool, the irradiation energy density of the laser beam may be gradually decreased from the vertically lower side of the molten pool toward the vertically upper side of the molten pool and may be gradually increased from the vertically upper side of the molten pool toward the vertically lower side of the molten pool. According to the present disclosure, it is possible to provide a laser welding method capable of suppressing the occurrence of welding failures when a plurality of stacked metal plates are welded in an upright position. The above and other objects, features and advantages of the present disclosure will become more fully understood from the detailed description given hereinbelow and the accompanying drawings which are given by way of illustration only, and thus are not to be considered as limiting the present disclosure.